Isover Rio Plus 2 x 6000 x 1200 x 50 mm, 14.4 mp glass mineral wool
Glass wool rolls 50 mm thickness 600 x 1200 mm (L x w) Advantages: fire safety, easy workability, excellent thermal insulation Roll with 2...
Glass mineral wool Isover Akusto Twin 7500 x 600 x 50, 18 sqm
Saltele de vata minerala de sticla 50 mm grosime 2 x 7500 x 600 mm (L x l) Avantaje: foarte buna atenuare a zgomotului, izolare termica...
Isover Uniroll Plus 10/5 2 x 5000 x 1200 x 50 mm 12mp
Compressed and rolled mattresses, made of glass mineral wool. The mattresses are obtained by melting the mineral raw materials in the oven, fibrillating the melting by the TEL process, applying a...
Isover Rio Plus 10/5 2 x 7000 x 1200 x 50 mm 16.8mp
Compressed and rolled mattresses, made of glass mineral wool. Mattresses are obtained by melting mineral raw materials in the oven, fibrilizing melting by the TEL process, applying a binder by...
Isover Akusto 7.5MPS 2 x 9000 x 600 x 75 mm Glass Wool 10.8mp
Compressed and rolled mattresses, made of glass mineral wool. Mattresses are obtained by melting mineral raw materials in the oven, fibrilizing melting by the TEL process, applying by spraying a...
Isover Domo Twin 10/5 2 x 6000 x 1200 x 50 mm 14.4mp
Compressed and rolled mattresses, made of glass mineral wool. Mattresses are obtained by melting mineral raw materials in the oven, fibrilizing melting by the TEL process, applying a binder by...
Isover Rio Alu 100 / 7500 x 1200 x 100 mm 9mp
Compressed and rolled mattresses, made of glass mineral wool. The mattresses are obtained by melting the mineral raw materials in the oven, fibrilizing the melting by the TEL process, applying a...
Isover Rio Alu 50 / 12000 x 1200 x 50 mm 14.4mp glass mineral wool
Compressed and rolled mattresses, made of glass mineral wool. The mattresses are obtained by melting the mineral raw materials in the oven, fibrilizing the melting by the TEL process, applying a...